Thermal annealing of bilayers of evaporated In on chemically deposited CdS thin films

In/CdS bilayers were prepared by evaporating In on CdS thin films deposited by the chemical bath technique. The thickness of the layers were about 50 and 150 nm for In and CdS respectively. In order to diffuse the In to the CdS layer, the bilayers were thermal annealed in air to temperatures from 25...