Effect of surface grain boundary density on preosteoblast proliferation on titanium
Studies since 2004 have shown that the cytocompatibility of ultrafine grain (UG) commercial purity (CP) titanium exceeds that of coarse grain (CG) CP titanium (Ti) by 30% to 20-fold. To isolate the factors affecting this large reported variability of CP titanium’s cytocompatibility, discs of UG and...