Modulus of Natural Rubber Cross-Linked by Dicumyl Peroxide II. Comparison With Theory
Thermodynamics and molecular considerations are applied to an examination of the equation G = S(fp + B)T + H(fp + B) + A = 5.925 × 10(−3)(fp − 0.45)T + 0.0684(fp − 0.45) + 2.70, found experimentally in Part I. G is the shear modulus in Mdyn cm(−2) at a temperature T for natural rubber cross-linked b...