Modulus of Natural Rubber Cross-Linked by Dicumyl Peroxide. I. Experimental Observations
Natural rubber mixed with varying amounts of dicumyl peroxide was cross-linked by heating 120 min at 149 °C. The quantitative measure of cross-linking was taken as the amount fp of decomposed dicumyl peroxide, the product of p, the number of parts added per hundred of rubber and f the fraction decom...