Compressibility of Natural Rubber at Pressures Below 500 kg/cm(2)

The specific volumes of unvulcanized natural rubber and of a peroxide-cured vulcanizate of natural rubber were measured at pressures of 1–500 kg/cm(2) at temperatures from 0 to 25 °C. Observations on mercury-filled dilatometers were made through a window in the pressure system. No time effects or hy...