Causes of Failure of Ceramic-on-Ceramic and Metal-on-Metal Hip Arthroplasties

BACKGROUND: Few large series of hard bearing surfaces have reported on reasons for early failure. A number of unique mechanisms of failure, including fracture, squeaking, and adverse tissue reactions, have been reported with these hard bearing surfaces. However, the incidence varies among the publis...