Carregant...

Causes of Failure of Ceramic-on-Ceramic and Metal-on-Metal Hip Arthroplasties

BACKGROUND: Few large series of hard bearing surfaces have reported on reasons for early failure. A number of unique mechanisms of failure, including fracture, squeaking, and adverse tissue reactions, have been reported with these hard bearing surfaces. However, the incidence varies among the publis...

Descripció completa

Guardat en:
Dades bibliogràfiques
Autors principals: Porat, Manny, Parvizi, Javad, Sharkey, Peter F., Berend, Keith R., Lombardi, Adolph V., Barrack, Robert L.
Format: Artigo
Idioma:Inglês
Publicat: Springer-Verlag 2011
Matèries:
Accés en línia:https://ncbi.nlm.nih.gov/pmc/articles/PMC3254760/
https://ncbi.nlm.nih.gov/pubmed/22045071
https://ncbi.nlm.nih.govhttp://dx.doi.org/10.1007/s11999-011-2161-y
Etiquetes: Afegir etiqueta
Sense etiquetes, Sigues el primer a etiquetar aquest registre!