Effect of Au Film Thickness and Surface Roughness on Room-Temperature Wafer Bonding and Wafer-Scale Vacuum Sealing by Au-Au Surface Activated Bonding
Au-Au surface activated bonding (SAB) using ultrathin Au films is effective for room-temperature pressureless wafer bonding. This paper reports the effect of the film thickness (15–500 nm) and surface roughness (0.3–1.6 nm) on room-temperature pressureless wafer bonding and sealing. The root-mean-sq...