With the process measures including KR pre-sulphurizing hot metal [S] ≤0.008% , to increase BOF preoxidizing adding aluminium amount from 0.010%-0.025% to 0.020%-0.035% , to increase adding Fe-Ca wire from 3.0 m/t to 4.0 m/t, LF refining time ≥35 min and white slag time ≥15 min , improving tundish s...