Production Practice of Avoiding Raw and Supplement Materials on Increase Carbon in MA Ultra-Low Carbon Steel Liquid during KB-150 t BOF-RH-CC Flowsheet
The production flowsheet for MA ultra-low carbon steel (/% : ≤0.005C, 0.007-0.012Si, 0.07-0.15Mn, ≤0.025P, ≤0.025S, ≤0.035Als, ≤0.0020N) is KB-150 t BOF (end [C] ≤0.020%)-RH-200 mm slab CC flowsheet. The effect of mold flux, tundish shielding agent and ladle refractory materials on incremental carbo...