QR Kodea

Degradation and fragmentation behavior of polypropylene and polystyrene in water

Abstract The polystyrene (PS) retrieved from the beach exhibited no change in surface texture. In contrast to it, the retrieved polypropylene (PP) had a rumpled surface texture. Highly reactive sulfate radical generated by K2S2O8 was employed as degradation initiator of PP and PS, and their degradat...

Deskribapen osoa

Gorde:
Xehetasun bibliografikoak
Egile Nagusiak: Hisayuki Nakatani, Yuina Ohshima, Taishi Uchiyama, Motokucho Suguru
Formatua: Artigo
Hizkuntza:Inglês
Argitaratua: Nature Portfolio 2022-11-01
Saila:Scientific Reports
Sarrera elektronikoa:https://doi.org/10.1038/s41598-022-23435-y
Etiketak: Etiketa erantsi