Degradation and fragmentation behavior of polypropylene and polystyrene in water
Abstract The polystyrene (PS) retrieved from the beach exhibited no change in surface texture. In contrast to it, the retrieved polypropylene (PP) had a rumpled surface texture. Highly reactive sulfate radical generated by K2S2O8 was employed as degradation initiator of PP and PS, and their degradat...
Salvato in:
| Autori principali: | , , , |
|---|---|
| Natura: | Artigo |
| Lingua: | Inglês |
| Pubblicazione: |
Nature Portfolio
2022-11-01
|
| Serie: | Scientific Reports |
| Accesso online: | https://doi.org/10.1038/s41598-022-23435-y |
| Tags: |
Nessun Tag, puoi essere il primo ad aggiungerne!!
|