Reoxidation control of refining slag and inclusion modification in TP347H stainless steel

The secondary oxidation caused by compositions of refining slag and Ca treatment on oxide inclusion was studied in TP347H stainless steel by EF+VOD+IC process. In industrial trials, the aluminum is used as the final deoxidation during VOD process. The FeO and SiO<sub>2</sub> contents in refining are...