Côd QR

Reoxidation control of refining slag and inclusion modification in TP347H stainless steel

The secondary oxidation caused by compositions of refining slag and Ca treatment on oxide inclusion was studied in TP347H stainless steel by EF+VOD+IC process. In industrial trials, the aluminum is used as the final deoxidation during VOD process. The FeO and SiO<sub>2</sub> contents in refining are...

Disgrifiad llawn

Wedi'i Gadw mewn:
Manylion Llyfryddiaeth
Prif Awduron: ZHANG Le-chen, BAO Yan-ping, WANG Min, ZHANG Chao-jie
Fformat: Artigo
Iaith:Chinês
Cyhoeddwyd: Science Press 2016-12-01
Cyfres:工程科学学报
Pynciau:
Mynediad Ar-lein:http://cje.ustb.edu.cn/article/doi/10.13374/j.issn2095-9389.2016.s1.001
Tagiau: Ychwanegu Tag
Dim Tagiau, Byddwch y cyntaf i dagio'r cofnod hwn!