Investigation of Cavitation Erosion, Microstructure, and Surface Topography of Hot-Rolled Magnesium-Based AZ 31B Alloys

Cavitation erosion is a phenomenon that causes the degradation of engineering components operating in fluids under oscillating pressure, and it occurs through the repeated implosion of cavitation bubbles adjacent to the solid surface. This complex phenomenon involves both the hydrodynamic factors of...