Código QR

Investigation of Cavitation Erosion, Microstructure, and Surface Topography of Hot-Rolled Magnesium-Based AZ 31B Alloys

Cavitation erosion is a phenomenon that causes the degradation of engineering components operating in fluids under oscillating pressure, and it occurs through the repeated implosion of cavitation bubbles adjacent to the solid surface. This complex phenomenon involves both the hydrodynamic factors of...

Descrición completa

Gardado en:
Detalles Bibliográficos
Principais autores: Claudia Ciurel, Ion Mitelea, Ilare Bordeașu, Dragoș Buzdugan, Corneliu Marius Crăciunescu, Ion-Dragoș Uțu
Formato: Artigo
Idioma:Inglês
Publicado: MDPI AG 2026-08-01
Series:Crystals
Assuntos:
Acceso en liña:https://www.mdpi.com/2073-4352/16/8/541