Deuterium retention in displacement-damaged tungsten-rhenium alloys: Influence of rhenium concentration and irradiation temperature
Tungsten (W) samples containing 0, 1, 3, and 5 at.% rhenium (Re) were irradiated by 20 MeV W ions to 0.5 dpa at 290 K and to 0.3 dpa at 1350 K. An additional set of samples was irradiated to 0.5 dpa at 290 K and then annealed at 1350 K. The irradiated samples were exposed to a deuterium (D) plasma a...
Guardat en:
| Autors principals: | , , , , , |
|---|---|
| Format: | Artigo |
| Idioma: | Inglês |
| Publicat: |
Elsevier
2024-12-01
|
| Col·lecció: | Nuclear Materials and Energy |
| Matèries: | |
| Accés en línia: | http://www.sciencedirect.com/science/article/pii/S2352179124001534 |
| Etiquetes: |
Sense etiquetes, Sigues el primer a etiquetar aquest registre!
|