Deuterium retention in displacement-damaged tungsten-rhenium alloys: Influence of rhenium concentration and irradiation temperature
Tungsten (W) samples containing 0, 1, 3, and 5 at.% rhenium (Re) were irradiated by 20 MeV W ions to 0.5 dpa at 290 K and to 0.3 dpa at 1350 K. An additional set of samples was irradiated to 0.5 dpa at 290 K and then annealed at 1350 K. The irradiated samples were exposed to a deuterium (D) plasma a...