XRD AND IR INVESTIGATIONS OF SOME COMMERCIAL POLYSTYRENE SAMPLES THERMALLY DEGRADED
Thermal degradation of commercial polystyrene was investigated by XRD and FT-IR methods. The samples were heated 30 minutes at temperatures 140ºC, 200ºC, 250ºC, 300ºC and 350ºC and then brought back to room temperature. XRD investigation denotes structural modification for samples heated above 200º...