QR kód

Mechanical Property and Microstructure of Rolled 7075 Alloy under Hot Compression with Different Original Grains

The hot compression of rolled 7075 alloys with different heat treatments was performed. The temperature ranged from 200 to 400 °C, and the strain rate was 0.01 s<sup>−1</sup>. The stress level decreases with the increasing temperature during compression, and the strength of the alloy in the original...

Celý popis

Uloženo v:
Podrobná bibliografie
Hlavní autoři: Tuo Ye, Sawei Qiu, Erli Xia, Fang Luo, Wei Liu, Yuanzhi Wu
Médium: Artigo
Jazyk:Inglês
Vydáno: MDPI AG 2023-08-01
Edice:Metals
Témata:
On-line přístup:https://www.mdpi.com/2075-4701/13/8/1456