Mechanical Property and Microstructure of Rolled 7075 Alloy under Hot Compression with Different Original Grains

The hot compression of rolled 7075 alloys with different heat treatments was performed. The temperature ranged from 200 to 400 °C, and the strain rate was 0.01 s<sup>−1</sup>. The stress level decreases with the increasing temperature during compression, and the strength of the alloy in the original...

Descripción completa

Guardado en:
Detalles Bibliográficos
Autores principales: Tuo Ye, Sawei Qiu, Erli Xia, Fang Luo, Wei Liu, Yuanzhi Wu
Formato: Artigo
Lenguaje:Inglês
Publicado: MDPI AG 2023-08-01
Colección:Metals
Materias:
Acceso en línea:https://www.mdpi.com/2075-4701/13/8/1456