Codi QR

Investigation of the effect of pressure, sintering temperature and time on silicon carbide microstructure

In this research, SiC ceramics were densified via spark plasma sintering (SPS) with 0.5wt.% B4C and 1.5wt.% C additions at temperatures ranging from 1900 to 2000°C for 5-65min under 10-50MPa applied pressure with an intermediate dwell at 1400°C, and the effects of applied pressure, sintering tempera...

Descripció completa

Guardat en:
Dades bibliogràfiques
Autors principals: Yasar Zeynep Ayguzer, DeLucca Vincent A., Haber Richard A.
Format: Artigo
Idioma:Inglês
Publicat: University of Novi Sad 2022-06-01
Col·lecció:Processing and Application of Ceramics
Matèries:
Accés en línia:https://doiserbia.nb.rs/img/doi/1820-6131/2023/1820-61312302189Y.pdf