Temperature Dependence and Microstructure Effects on Magnetic Properties of FePt(B, Ag, C) Film

A FePt(B, Ag, C) granular film was formed from post-annealed B(4)C(1.0 nm)/FePt(Ag, C) layers at a substrate temperature of 470 °C for 2 min. The 6 nm thick FePt(B, Ag, C) film demonstrates high perpendicular magnetic anisotropy (K(u) = 2.83 × 10(7) erg/cm(3) at 100 K) and out-of-plane coercivity (H...