How Single-Walled Carbon Nanotubes are Transformed into Multiwalled Carbon Nanotubes during Heat Treatment
[Image: see text] High-pressure carbon monoxide (HiPCO) single-walled carbon nanotubes (SWCNTs) were heat treated at high temperatures from 1700 to 3000 °C. During the heating below 2500 °C, the diameters of the SWCNTs gradually increase from ∼1.0 to >1.5 nm, and at the temperatures higher than 2...