Investigation on the Corrosion of the Elbows in the Flue Gas Cooler of a 600 MW Coal-Fired Power Plant

[Image: see text] Sulfuric acid condensation has long been considered as the major cause of the corrosion issues at the cold-end of coal-fired boilers. However, in a flue gas cooler, where flue gas is cooled to around 90 °C for heat recovery, the influence of chlorides might be underestimated. In th...