Autogenous Fiber Laser Welding of 316L Austenitic and 2304 Lean Duplex Stainless Steels

This study presents results of experimental tests on quality of dissimilar welded joints between 316L austenitic and 2304 lean duplex stainless steels, welded without ceramic backing. Fiber laser welded butt joints at a thickness of 8 mm were subjected to non-destructive testing (visual and penetran...