Shear Bond Strength of Ceramic Bonded to Different Core Materials and Their Pattern of Failure: An In Vitro Study

Introduction In metal-ceramic restoration, most of the bond failures between the ceramic layer and the metal coping is the chipping of the ceramic layer, thus exposing the metal surface, which compromises the aesthetics. Hence, this leads to the introduction of zirconia-based restorations in dentist...