Effects of Microwave Sintering Temperature and Holding Time on Mechanical Properties and Microstructure of Si(3)N(4)/n-SiC ceramics

The n-SiC (nanometer SiC) is added to be the additive in order to improve the mechanical performance of Si(3)N(4) ceramics. A microwave sintered the ceramics at different temperature and holding times. The results shows that the Si(3)N(4)/n-SiC ceramics (85 wt% Si(3)N(4) + 5 wt% n-SiC + 5 wt% Al(2)O...