Study on Crystallization Behaviors and Properties of F-III Fibers during Hot Drawing in Supercritical Carbon Dioxide

In order to obtain F-III fibers with high mechanical properties, pristine F-III fibers were hot drawn at the temperature of 250 °C, pressure of 14 MPa, tension of 6 g·d(−1), and different times, which were 15 min, 30 min, 45 min, 60 min, 75 min, 90 min, and 105 min, respectively, in supercritical ca...