Crystal orientation-dependent fatigue characteristics in micrometer-sized single-crystal silicon

Repetitive bending fatigue tests were performed using five types of single-crystal silicon specimens with different crystal orientations fabricated from {100} and {110} wafers. Fatigue lifetimes in a wide range between 10(0) and 10(10) were obtained using fan-shaped resonator test devices. Fracture...