Enhanced Stretch Formability of AZ31 Magnesium Alloy Thin Sheet by Induced Precompression and Sequent Annealing
In this study, precompression deformation with a strain level of 5.38% along the transverse direction (TD) at room temperature was conducted on a AZ31 magnesium alloy thin sheet with thickness of 1mm. Then subsequent annealing treatment was carried out at various temperatures (200, 300, 400, and 500...