Carregant...

Dataset on the microstructure Ni(50)Mn(38)Sb(9)Si(3) alloy and compositions of Ni(50)Mn(38)Sb(12−x)Si(x) (x=2.5, 3) ferromagnetic shape memory alloys

The data presented in this article is the supplementary data of Zhang et al. (2018) [1]. The Ni(50)Mn(38)Sb(9)Si(3) alloy is annealed at 1223 K for 24 h and then quenched into ice water; while the Ni(50)Mn(38)Sb(9.5)Si(2.5) alloy is annealed at 1173 K for 24 h and then quenched into ice water. The m...

Descripció completa

Guardat en:
Dades bibliogràfiques
Publicat a:Data Brief
Autors principals: Zhang, Ruochen, Zhang, Xuexi, Qian, Mingfang, Sun, Jianfei, Geng, Lin
Format: Artigo
Idioma:Inglês
Publicat: Elsevier 2018
Matèries:
Accés en línia:https://ncbi.nlm.nih.gov/pmc/articles/PMC5993163/
https://ncbi.nlm.nih.gov/pubmed/29892636
https://ncbi.nlm.nih.govhttp://dx.doi.org/10.1016/j.dib.2018.05.002
Etiquetes: Afegir etiqueta