Fabrication of Zr(2)WP(2)O(12)/ZrV(0.6)P(1.4)O(7) composite with a nearly zero-thermal-expansion property

Sintered bodies of Zr(2)WP(2)O(12) (ZWP) and ZrV(0.6)P(1.4)O(7) (ZVP) were fabricated, and their linear thermal expansion coefficients (TEC) were found to be −2.92 × 10(−6) and 3.27 × 10(−6) °C(−1), respectively, in the range 25–500 °C. In an attempt to fabricate composites with a zero-thermal-expan...