Properties of Foamed Mortar Prepared with Granulated Blast-Furnace Slag

Foamed mortar with a density of 1300 kg/m(3) was prepared. In the initial laboratory trials, water-to-cement (w/c) ratios ranging from 0.54 to 0.64 were tested to determine the optimal value for foamed mortar corresponding to the highest compressive strength without compromising its fresh state prop...