Nanostructured laminar tungsten alloy with improved ductility by surface mechanical attrition treatment

A nanostructured laminar W-La(2)O(3) alloy (WL10) with improved ductility was prepared using a surface mechanical attrition treatment (SMAT). φ1.5 mm ZrO(2) WL10 balls subjected to SMAT (called φ1.5 mm ZrO(2) ball SMATed WL10) samples possess the best surface profile and excellent integrated mechani...