Thermal Degradation of Fractionated High and Low Molecular Weight Polystyrenes
In previous work on the thermal degradation of polystyrene of average molecular weight of 230,000, carried out in a vacuum in the temperature range 318 to 348 °C, the rate curves exhibited distinct maximums when percentage loss of sample per minute was plotted as a function of percentage volatilizat...