Evidence for the transition from primary to peritectic phase growth during solidification of undercooled Ni-Zr alloy levitated by electromagnetic field
The Ni(83.25)Zr(16.75) peritectic alloy was undercooled by electromagnetic levitation method up to 198 K. The measured dendritic growth velocity shows a steep acceleration at a critical undercooling of ΔT(crit) = 124 K, which provides an evidence of the transition of the primary growth mode from Ni(...