Evaluation of enamel surface modification using PS-OCT after laser treatment to increase resistance to demineralization

At laser intensities below ablation, carbonated hydroxyapatite in enamel is converted into a purer phase hydroxyapatite with increased acid resistance. Previous studies suggested the possibility of achieving the conversion without surface modification. This study attempts to evaluate the thresholds...