Thin Hard Crest on the Edge of Ceramic Acetabular Liners Accelerates Wear in Edge Loading
Ceramic acetabular liners may exhibit a small, sharp crest - an artifact of discontinuous machining steps - at the junction between the concave spherical surface and the interior edge. On three ceramic liners, this crest was found to form a 9–11° deviation from tangency. Edge loading wear tests were...