Codice QR

Preparation of 125I Radioactive Covered Metal Stent

Using Polyisocyanate as cross linking agent, preparation of 125I radioactive covered metal stent with polyurethane. The dipping times, solution concentration of polyurethane and time of dipping on the coating thickness were studied. The membrane thickness was 7.9 μm. The specimens from 30 days after...

Descrizione completa

Salvato in:
Dettagli Bibliografici
Autore principale: CHEN Zhen1,2;CHEN Ya-hong1,2;LI Wei1,2
Natura: Artigo
Lingua:Chinês
Pubblicazione: Editorial Board of Journal of Isotopes 2014-02-01
Serie:Journal of Isotopes
Soggetti:
Accesso online:http://www.tws.org.cn/CN/10.7538/tws.2014.27.02.0109