Process Practice for Production of Steel H11Mn2SiA for Welding Wire by 65 t Consteel EBT EAF-LF-CC Flowsheet at Shiheng Steel
With using 60% hot metal + quality scrap charge,Consteel EAF eccentric bottom tapping operation,con- trolling tapping end [C] 0.035%~0.050% and tapping[P]≤0.012%,LF refining by low basicity slag,feeding silicon wire, soft blown argon for 15 min afte...