Control of Nitrogen Content in Bearing Steel Steelmaking by a 50 t EAF-LF(VD)-CC Flowsheet
The nitrogen content in GCr15 bearing steel at each melting phase in 50 t EAF-LF(VD)-CC process was analyzed to obtain that the EAF end [N] was(23~36)×10-⁶ and the N content in products was (79~104)×10-⁶.In order to decrease the N content in bearing steel, with charging ≥35% hot metal in EAF, using...