Damage Mechanism of HgCdTe Focal Plane Array Detector Irradiated Using Mid-Infrared Pulse Laser

To investigate the damage threshold and mechanism of a mid-infrared HgCdTe focal plane array (FPA) detector, relevant experimental and theoretical studies were conducted. The line damage threshold of a HgCdTe FPA detector may be within the range of 0.59 Jcm<sup>−2</sup> to 0.71 Jcm<sup>−2</sup>. The...