Microstructure and Mechanical Properties of TiAl Alloy Prepared by Spark Plasma Sintering

The Ti43. 5Al5Nb1V1Y ( at. % ) prealloyed powder prepared by the gas atomization process was used as the raw material,and the fine grained TiAl alloy was successfully prepared by the spark plasma sintering process. The effects of different sintering temperatures ( 1,200 ~ 1,300℃ ) on the microstruct...