Joining Of Green Body And Dense Substrate For Indium Tin Oxide Under Uniaxial Pressure In An Open Condition

The green body and dense substrate of indium tin oxide was joined by uniaxially pressing at 0.3 MPa at 1300°C to test the restoring of the eroded part of transparent conducting oxide target. The green body was sintered to 98% of theoretical density under the suppression of shrinkage along the bounda...