Microstructure and properties degradation of P/T 91, 92 steels weldments in creep conditions

The studies were performed on dissimilar ferritic/austenitic weldments between 9Cr tempered martensitic steels of the grades either P/T 91 or 92 and unstabilised AISI316H austenitic steel. The welded joints were fabricated using the fusion welding by tungsten inert gas (TIG) method with Ni-based...