Effect of LF(VD)Refining Process on Control of Sulphur and Sulphide in Gear Steel 28MnCr5
The basicity of refining slag,feeding sulphur wire and deoxidation process for a 45 t LF on control of sulphur,oxide content and sulphide in steel 28MnCr5(0.25~0.30C,0.60~0.80Mn,0.020~0.035S,0.80~1.00Cr) have been tested. Results showed that as feeding sulphur wire with basicity of LF refining s...