Effect of low temperature on early strength of cemented paste backfill from a copper mine and engineering recommendations

Low winter temperatures are a widespread concern for mines in China that use cemented paste backfill (CPB). A low environmental temperature has a significant effect on the CPB temperature, which can affect its hydration rate and early strength. Using paste material from the Jiashi Copper Mine (JCM)...