The spring steel SK5 (/% : 0.75 ~0. 84C,≤ 0. 35Si, ≤0.40Mn, ≤0. 035P, ≤0.030S) is produced by 100 t EAF-LF-VD-CC flow sheet. With using the process measures including pre-deoxidizing at EAF tapping by adding silicon-manganese and ferroaluminium, compound-deoxi dizing during LF refining process by ad...