Código QR

Interfacial microstructure and corrosion behavior of ODS FeCrAl alloy in oxygen-saturated lead-bismuth eutectic at 450 °C

Abstract The interfacial microstructure and corrosion behavior of oxide dispersion strengthening (ODS) FeCrAl alloy with 20 wt% Cr (e.g. 20Cr ODS FeCrAl alloy) exposed to static oxygen-saturated lead-bismuth eutectic (LBE) at 450 °C for 20 h, 40 h, 60 h, 80 h and 100 h as exposure time respectively...

Descrición completa

Gardado en:
Detalles Bibliográficos
Principais autores: Yang Luo, Shengqiang Ma, Ping Lv, Yusheng Liu, Xiaoting Wang, Liangliang Lv, Jiandong Xing
Formato: Artigo
Idioma:Inglês
Publicado: Nature Portfolio 2024-10-01
Series:Scientific Reports
Assuntos:
Acceso en liña:https://doi.org/10.1038/s41598-024-77786-9